soghra salehi; M. Noaparast; S.Z. Shafaei; A. Amini; A. Heidarnia
Abstract
In this work, hydrochloric acid is used to remove iron impurities in the bauxite ore contained in the diasporite mineral located in the Sari region. The bauxite ore was calcined at different temperatures and times, and then dissolved in a hydrochloric acid solution. After determining the optimum calcination ...
Read More
In this work, hydrochloric acid is used to remove iron impurities in the bauxite ore contained in the diasporite mineral located in the Sari region. The bauxite ore was calcined at different temperatures and times, and then dissolved in a hydrochloric acid solution. After determining the optimum calcination conditions in 1 h at 900 °C, the response surface methodology (RSM) with four factors in five levels was employed in order to evaluate the effects of calcination temperature, calcination time, acid concentration, and leaching time on the iron leaching efficiency. A quadratic model is proposed using this methodology to correlate the leaching variables. The test results indicate that the model is consistent with the experimental data, and that the most important varriables involved are the acid concentration, leaching time, and squared term of calcination temperature (A2). The maximum iron recovery was 94.97%, and the Fe grade in the solids remained was 2.35% at the calcination temperature of 900 °C, a calcination time of 1 hour, and a leaching time of 2 h in hydrochloric acid (6 mM).
Z. Bahri; S.Z. Shafaei; M. Karamoozian
Abstract
Investigations were carried out on coal tailings by conventional cell and column flotation techniques. Tests were conducted to assess processing coal tailings of Alborz Markazi coal washing plant in Iran by column flotation. The effects of reagent type/dosage were investigated with conventional flotation ...
Read More
Investigations were carried out on coal tailings by conventional cell and column flotation techniques. Tests were conducted to assess processing coal tailings of Alborz Markazi coal washing plant in Iran by column flotation. The effects of reagent type/dosage were investigated with conventional flotation and their results were used in the performance of column flotation. Also the effects of the air rate, the feeding rate, the wash water rate, the frother concentration, the collector dosage were evaluated with column flotation. These coal tailings have an average of 56% ash. This paper used factorial design to optimize grade and recovery of coal tailings. The column flotation results indicated concentrate produced under optimum conditions, kerosene, 2909 g/t; superficial air velocity, 0.96 cm/s; feeding rate, 3.6 lit/min; superficial wash water velocity, 0.98 lit/min; frother dosage, 350 g/t having an ash content of 12.11% and a combustible recovery of 28.51% was obtained.